Hoge sterkte Inconel 718 Precipitatiehardbare nikkel-chroom-superlegering
Basis eigenschappen
Plaats van herkomst:
GEMAAKT IN CHINA
Merknaam:
Baosteel,TISCO
Certificering:
EN 10204 Type 3.1 / 3.2 available
Modelnummer:
Incoloy 800 / Incoloy 800H / Incoloy 800HT / Incoloy 825 / Hastelloy C-276 / Hastelloy C-22 / Inco
Handelsgoederen
Minimale bestelhoeveelheid:
100 kg
Prijs:
Negotiable (Request a Quote)
Betalingsvoorwaarden:
T/T, D/P, D/A, Western Union, PayPal
Leveringscapaciteit:
10000TONS
Gerelateerde producten
-
Precision 301 304 316 430 koudgewalst roestvrij staal band 2B BA No.4 Afwerking
Precision cold rolled stainless steel strip is a narrow, thin-gauge stainless steel product manufactured to significantly tighter thickness and width tolerances than standard cold-rolled sheet. Unlike standard sheet (typically 1000mm or 1219mm wide), precision strip is produced in narrow widths — usually less than 600mm — and thin gauges from 0.05mm up to 3.0mm. The key differentiator is the tolerance : the precision strip holds thickness variations to as low as ±0.005mm, -
Hoge precisie 304 roestvrij staal naadloos buis koudgewalste corrosiebestendigheid
304 Stainless Steel Seamless Pipe The 304 stainless steel seamless pipe is a globally recognized standard grade in the stainless steel family. With a chemical composition of 18% chromium and 8% nickel, it offers excellent corrosion resistance, high toughness, and outstanding formability. Manufactured using precision seamless cold-rolling technology, this pipe delivers a superior surface finish, tight dimensional tolerances, and consistent mechanical properties — making it the -
UNS N06022 Hastelloy C-22 legering corrosiebestendig ASTM B622
UNS N06022 is a nickel-chromium-molybdenum alloy renowned for its exceptional resistance to both oxidizing and reducing corrosive media. With a higher chromium content than C-276, plus controlled additions of tungsten, this alloy offers superior resistance to pitting, crevice corrosion, and stress-corrosion cracking in aggressive environments. UNS N06022 provides outstanding performance in wet chlorine, hydrochloric acid, sulfuric acid, and mixed acid solutions where many -
Austenitische corrosiebestendige Hastelloy C-22 nikkellegering voor zware chemische verwerking
Hastelloy C-22: Ultimate Corrosion-Resistant Nickel Alloy Hastelloy C-22 is a fully austenitic, advanced corrosion-resistant nickel-chromium-molybdenum-tungsten alloy. It offers outstanding resistance to both uniform corrosion in oxidizing media and localized attack (pitting, crevice corrosion) in reducing environments. Unlike standard alloys, C-22 provides exceptional resistance to stress corrosion cracking (SCC), intergranular attack, and weld heat-affected zone (HAZ)